折疊和麻面是nd鋼管常見的表面缺陷類型,容易造成成材報廢,影響nd鋼管的金屬收得率,需要分清表面質(zhì)量缺陷的類型及分析其成因,并采取行之有效的控制措施。對于兩者的常見情況及控制措施為:
Folding and hemp surface are common surface defects of ND steel pipe, which easily lead to scrap of finished products and affect metal yield of ND steel pipe. It is necessary to distinguish the types of surface quality defects and analyze their causes, and take effective control measures. The common situations and control measures are as follows: 1折疊。
1 fold.
折疊指nd鋼管的表面沿軋制方向成直線狀或鋸齒狀裂紋。情況為:連續(xù)或斷續(xù)出現(xiàn)在nd考登鋼管局部或全長,深淺不一,內(nèi)有氧化鐵皮的橫斷面上經(jīng)扭轉(zhuǎn)呈折面翹起。直線狀的折疊與法裂、劃痕相似,通過挫平斷面或作扭轉(zhuǎn)實驗可以區(qū)別。
Folding refers to the straight or serrated cracks on the surface of ND steel pipe along the rolling direction. Circumstances are as follows: continuous or intermittent appearance in part or full length of ndkauden steel pipe, varying in depth, with iron oxide scales in the cross section of the torsion is folded upward. Linear folding is similar to normal cracking and scratches. It can be distinguished by frustrating the section or doing torsion experiments.
控制措施為:精細(xì)操作,防止各道孔型出現(xiàn)耳子,造成后續(xù)折疊;認(rèn)真檢查輥環(huán)、軋槽的使用情況,及時更換;嚴(yán)格檢驗原料質(zhì)量,對缺陷必須徹底清理后才可入爐。
The control measures are as follows: fine operation to prevent ears from appearing in each pass and subsequent folding; careful inspection of the use of roll rings and rolling grooves, timely replacement; strict inspection of raw material quality, and thorough cleaning of defects before entering the furnace.
2麻面。
2 pock.
麻面指nd鋼管表面上有許多細(xì)小凹點組成的片狀粗糙面。情況為:在nd考登鋼管的全長連續(xù)或周期出現(xiàn)。
The hemp surface refers to the flaky rough surface formed by many small concave points on the surface of ND steel pipe. The situation is as follows: the whole length of ndkauden steel tube appears continuously or periodically.
Folding and hemp surface are common surface defects of ND steel pipe, which easily lead to scrap of finished products and affect metal yield of ND steel pipe. It is necessary to distinguish the types of surface quality defects and analyze their causes, and take effective control measures. The common situations and control measures are as follows: 1折疊。
1 fold.
折疊指nd鋼管的表面沿軋制方向成直線狀或鋸齒狀裂紋。情況為:連續(xù)或斷續(xù)出現(xiàn)在nd考登鋼管局部或全長,深淺不一,內(nèi)有氧化鐵皮的橫斷面上經(jīng)扭轉(zhuǎn)呈折面翹起。直線狀的折疊與法裂、劃痕相似,通過挫平斷面或作扭轉(zhuǎn)實驗可以區(qū)別。
Folding refers to the straight or serrated cracks on the surface of ND steel pipe along the rolling direction. Circumstances are as follows: continuous or intermittent appearance in part or full length of ndkauden steel pipe, varying in depth, with iron oxide scales in the cross section of the torsion is folded upward. Linear folding is similar to normal cracking and scratches. It can be distinguished by frustrating the section or doing torsion experiments.
控制措施為:精細(xì)操作,防止各道孔型出現(xiàn)耳子,造成后續(xù)折疊;認(rèn)真檢查輥環(huán)、軋槽的使用情況,及時更換;嚴(yán)格檢驗原料質(zhì)量,對缺陷必須徹底清理后才可入爐。
The control measures are as follows: fine operation to prevent ears from appearing in each pass and subsequent folding; careful inspection of the use of roll rings and rolling grooves, timely replacement; strict inspection of raw material quality, and thorough cleaning of defects before entering the furnace.
2麻面。
2 pock.
麻面指nd鋼管表面上有許多細(xì)小凹點組成的片狀粗糙面。情況為:在nd考登鋼管的全長連續(xù)或周期出現(xiàn)。
The hemp surface refers to the flaky rough surface formed by many small concave points on the surface of ND steel pipe. The situation is as follows: the whole length of ndkauden steel tube appears continuously or periodically.
上一篇:沒有了
下一篇:如何判斷nd鋼管外面有沒有氧化皮
推薦資訊
- 2020-05-18翅片管的主要功能
- 2020-05-18翅片管的功能包含哪些方面?
- 2020-05-18在我們生活中選購翅片管的六個要點
- 2020-05-18現(xiàn)在的激光焊翅片管的種類多且技術(shù)先進(jìn)
- 2020-05-18解析激光焊翅片管的換熱元件及使用方式
- 2020-05-16對ND鋼管一般斑點狀偏析的成因分析
- 2020-05-16考登鋼管的合金成分及重量百分比含量
- 2020-05-16考登管的主要生產(chǎn)材質(zhì)及綜合用途
- 2020-05-16考登鋼管與ND鋼管的異同點
- 2020-05-16考登管的常見用途于分類
推薦產(chǎn)品